9:00 AM-10:30 AM Metro Toronto Convention Centre Room 801A, Oral |
Keynote Address and Cytotoxicity of Restorative Materials |
Chairpersons: A. SCHEDLE and A. SENGUN |
| |
| 0131 |
| Keynote Address: Standardization of Biocompatibility Testing of Dental Materials G. SCHMALZ, University of Regensburg, Germany |
| 0132 |
| Cytotoxicity of dental bonding substances as a function of Degree-of-Conversion A. FRANZ1, F. KÖNIG2, D.C. WATTS3, and A. SCHEDLE1, 1Bernhard Gottlieb University Clinic of Dentistry, Vienna, Austria, 2Medical University of Vienna, Austria, 3University of Manchester, United Kingdom |
| 0133 |
| Evaluation of Cytotoxicity and Degree of Conversion of Orthodontic Adhesives N. JAGDISH, Shri Ramachandra Dentl College, Chennai, MD, India |
| 0134 |
| Cytotoxic Effects of Glass Ionomer Cements on Bovine Pulp-Derived Cells A. SENGUN1, H.E. BOTSALI1, M. YALCIN1, F. OZER1, and S.S. HAKKI2, 1Selcuk University, Department of Operative Dentistry, Konya, Turkey, 2Selcuk Universitesi, Department of Periodontology, Konya, Turkey |
| 0135 |
| Targeted Compounds Released from Resin-Based Dental Materials F. MORAN, Cardiff University, AL, United Kingdom, R.J. WADDINGTON, Cardiff University, Wales, and A.S.M. GILMOUR, Cardiff University, United Kingdom |
|
Back to the: Dental Materials 4: Clinical Trials, Biocompatibility and Biologic Effects Program
|
|