1:45 PM-3:00 PM Metro Toronto Convention Centre Exhibit Hall D-E, Poster |
Ceramic Fatigue and Fracture, Color, and Others |
| |
| 3143 | Effect of veneering techniques on damage and reliability of Y-TZP-trilayers P. GUESS, Y. ZHANG, and V.P. THOMPSON, New York University, USA |
| 3144 | Failure modes of veneering porcelain supported by alumina-substructures B. KIM, M. PINES, D. STAPPERT, V.P. THOMPSON, and C.F. STAPPERT, New York University, USA |
| 3145 | Cyclic Fatigue Behaviour of Glass-Infiltrated Ceramics Under Different Environments S.M. SALAZAR MAROCHO, Universidade Est. Paulista Julio Mesquita, Sao Paulo, Brazil, A.R. STUDART, Harvard University, Cambridge, MA, USA, M.A. BOTTINO, Universidade Est. Paulista Julio Mesquita, São José dos Campos, Brazil, and A. DELLA-BONA, University of Passo Fundo, Passo Fundo, RS, Brazil |
| 3146 | Fracture Behavior of In-Ceram® Zirconia CAD/CAM Substructures Under Cyclic Fatigue R.F. ANDREIUOLO1, C.E. SABROSA2, C. FILGUEIRAS1, F.T. SILVA1, R. POBER3, and R. GIORDANO3, 1Universidade Federal do Rio de Janeiro, Niterói, Rio de Janeiro, Brazil, 2Universidade do estado do Rio de Janeiro, Brazil, 3Boston University, MA, USA |
| 3147 | Effect of air-particle-abrasion on cyclic and flexural strength of zirconia R.M. MELO, Sao Paulo State University, Sao Jose dos Campos, Brazil, M. ÖZCAN, University of Groningen, Netherlands, R.O.A. SOUZA, Sao Paulo State University (Unesp/SJC), Sao Jose dos Campos, Brazil, K.M.C. OLIVEIRA, State University of Campinas (UNICAMP), Piracicaba, Brazil, L.F. VALANDRO, Federal University of Santa Maria, Brazil, and M.A. BOTTINO, São Paulo State University (UNESP), São José dos Campos, Brazil |
| 3148 | Ceramic ion exchange: effect in strength and slow crack growth V. ROSA1, M.M. PINTO2, C.C. GONZAGA3, P.F. CESAR3, and H.N. YOSHIMURA4, 1University São Paulo, Passo Fundo - RS, Brazil, 2University of São Paulo, São Paulo - SP, Brazil, 3University of Sao Paulo, Brazil, 4Institute of Technological Research of the State of São Paulo, Brazil |
| 3149 | Visualization of Transformation Toughening for Newly Developed Ce-TZP/Alumina Nanocomposite M. NAWA1, Y. SUEHIRO1, H. NAKANISHI1, K. YAMADA2, and G. PEZZOTTI2, 1Matsushita Electric Works, Ltd, Osaka, Japan, 2Kyoto Institute of Technology, Japan |
| 3150 | Testing Methods to Determine the Shear-Bond-Strength of Veneering-Porcelain to Zirconia F. BEUER, Munich Dental School, Munchen, Germany, and J.A. SORENSEN, Pacific Dental Institute, Portland, OR, USA |
| 3151 | Ceramic Base Crown Near-net-shape Using Gel-casting Technique J. MA1, S. WANG1, W. WANG1, R. DU1, and X. LI2, 1Wenzhou Medical College, Wenzhou, Zhejiang, China, 2Sichuan University, Chengdu, Sichuan, China |
| 3152 | Chemical Activators on Fluorescence of Dental Ceramics J.-B. SU, T.-M. WANG, and L.-D. LIN, National Taiwan University, Taipei, Taiwan |
| 3153 | Surface Change of Zirconia by Nd:YAG Laser Irradiation S. BAN1, Y. MINESAKI1, and Y. TAKENOUCHI2, 1Kagoshima University, Japan, 2A-Dental Labo, Kagoshima, Japan |
| 3154 | Translucency Comparison of CAD/CAM Materials R. ALKHUNAIZI, R. POBER, and R. GIORDANO, Boston University, MA, USA |
| 3155 | Colour correspondence of ceramic systems in two different shade guides A. VICHI1, G. CORCIOLANI2, C. GORACCI3, and M. FERRARI2, 1Siena University, Grosseto, Italy, 2University of Siena, Italy, 3Department of Fixed Prostodontics and Dental Materials, University of Siena, Italy, Grosseto, Italy |
|
Back to the: Dental Materials 3: Ceramic-based Materials and Cements Program
|
|